机械合金化与包套快锻制备Ni6Cr4W1Fe9Ti2高熵合金块材的组织与性能

*通信作者, E-mail: fuzeng.a.chang@cisdi.com.cn

  • 摘要: 面向沿海服役飞机起落架连接件的氯盐腐蚀防护需求,本文先通过机械合金化获得Ni?Cr?W?Fe?Ti?粉末,再经等离子熔喷球化及包套快锻制得块体材料,并考察棒料比、退火条件和烧结制度对其组织与性能的作用。结果显示,在60∶1棒料比下研磨8 h后,粉末形成FCC+BCC双相固溶体,合金化程度较高且Fe污染较少;温度超过800 ℃后BCC相逐步向FCC相转化,960 ℃退火样品以FCC相为主并伴有少量TiC。升高烧结温度或增加保温时间均有利于致密化,相对密度最高达到98.1%。采用1200 ℃、6 h烧结时,样品抗压强度达到2013 MPa,压缩率为42.45%;在3.5 wt.% NaCl溶液中测得自腐蚀电流密度102 nA·cm?2、极化电阻373.85 kΩ·cm2,其耐蚀表现接近于同条件下的304不锈钢。

     

    Abstract: To meet the demand for resistance to chloride-induced corrosion in connecting components of coastal aircraft landing gear, a Ni?Cr?W?Fe?Ti? high-entropy alloy was fabricated through mechanical alloying, plasma melt-spray spheroidization, and canned rapid forging. The effects of the rod-to-powder ratio, annealing treatment, and sintering schedule on the microstructure and properties of the alloy were investigated. The results showed that, at a rod-to-powder ratio of 60:1, the powder evolved into an FCC+BCC dual-phase solid solution after 8 h of milling, exhibiting a relatively high degree of alloying and low Fe contamination. The BCC-to-FCC phase transformation began above 800 °C. After annealing at 960 °C, the alloy consisted primarily of an FCC phase with a small amount of TiC. Increasing the sintering temperature and prolonging the holding time promoted densification, yielding a maximum relative density of 98.1%. The sample sintered at 1200 °C for 6 h exhibited a compressive strength of 2013 MPa and a compressive strain of 42.45%. In a 3.5 wt.% NaCl solution, the sample showed a corrosion current density of 102 nA·cm?2 and a polarization resistance of 373.85 kΩ·cm2,it’s corrosion resistance performance is close to 304 stainless steel under the present experimental conditions.

     

/

返回文章
返回