分层交替扫描速度对激光定向能量沉积TA15钛合金增塑机制研究

Study on the plasticizing mechanism of laser directed energy deposition of TA15 titanium alloy by layered alternating scanning speed

  • 摘要: 针对激光定向能量沉积(L-DED)TA15钛合金沉积态组织中粗大柱状β晶连续外延生长、织构明显和塑性不足的问题,以及目前研究多聚焦于不同合金成分复合制备双金属结构与单一工艺参数塑性较低的局限性下,本研究提出一种采用600、900、1200 mm/min恒定扫描速度和600×900 mm/min分层交替扫描速度制备TA15钛合金试样的方法。结果表明,恒定扫描速度试样中原始β晶粒主要沿沉积方向连续外延生长,形成贯穿多层的柱状晶;分层交替扫描速度试样通过周期性改变熔池热输入,使前一层顶部CET等轴晶区得以部分保留,从而阻断β晶粒连续外延生长并促进近等轴化。分层交替扫描速度试样的α片层平均厚度降至0.271 μm,形成致密交错的超细网篮组织。室温拉伸结果显示,600×900 mm/min试样的断裂伸长率达到12.9%,相较于三种恒定扫描速度试样分别提高43.3%、53.6%和69.7%。在维持较高强度水平的前提下显著提升塑性,实现强塑性综合优化提升主要源于近等轴β晶粒削弱织构并改善变形协调性,超细α网篮组织通过密集界面提升强度与抗裂性,周期性热应力激活<c+a>全位错以增强c轴变形能力,弥散纳米β相通过异质变形强化维持加工硬化并缓解应力集中。该结果为L-DED TA15钛合金在不改变成分条件下实现塑性提升优化提供了可行工艺路径。

     

    Abstract: To address the issues of continuous epitaxial growth, obvious texture, and insufficient plasticity of coarse columnar β crystals in the deposited microstructure of laser directed energy deposition (L-DED) TA15 titanium alloy, and the limitations of current research focusing on bimetallic structures prepared by composite different alloy compositions and the low plasticity of single process parameters, this study proposes a method for preparing TA15 titanium alloy specimens using constant scanning speeds of 600, 900, and 1200 mm/min and alternating layered scanning speeds of 600×900 mm/min. Results show that in the constant scanning rate samples, the original β grains mainly grow continuously along the deposition direction, forming columnar crystals that penetrate multiple layers; The layered alternating scanning speed samples periodically change the heat input of the melt pool, partially preserving the CET equiaxed crystal region at the top of the previous layer, thereby blocking continuous epitaxial growth of β grains and promoting near-equiaxation. The average thickness of the α layer thickness of the layered alternating scanning speed samples dropped to 0.271 μm,forming a dense and interlaced ultrafine mesh basket microstructure. Room temperature tensile results showed that the elongation at break of 600×900 mm/min reached 12.9%, an increase of 43.3%, 53.6%, and 69.7% compared to the three constant scanning speed samples. Significantly improving plasticity while maintaining a high strength level to achieve the comprehensive optimization of strength and plasticity mainly stems from the near-equiaxed β grains weakening the texture and improving deformation coordination. The ultrafine α mesh basket microstructure enhanced strength and crack resistance through dense interfaces, periodic thermal stress activated <C+A> total dislocations to enhance c-axis deformation capability, and the dispersed nano β phase maintains work hardening and alleviated stress concentration through heteromorphic deformation. This result provides a feasible process route for improving and optimizing the plasticity of L-DED TA15 titanium alloy without changing its composition.

     

/

返回文章
返回