高级检索

钼合金表面梯度抗氧化涂层研究进展

Research progress on gradient oxidation-resistant coatings for molybdenum alloys

  • 摘要: 钼合金在600 °C以上即因三氧化钼挥发而发生严重氧化损耗,表面防护涂层是保障其高温服役寿命的关键途径。然而,现有抗氧化涂层与钼合金基体热膨胀系数差异导致涂层与基体界面开裂。因此,常围绕热膨胀匹配、元素扩散控制、保护膜形成与再生的核心设计钼合金表面梯度抗氧化涂层,实现抗氧化涂层的长周期稳定服役。本文综述了钼合金表面梯度抗氧化涂层的研究进展,将现有梯度涂层划分两个层次五个框架:第一层次梯度骨架构筑路径包括阶梯式扩散梯度涂层、纳米梯度涂层和原位生成复合梯度涂层;第二层次在梯度骨架上实施的复合改性路径包括第二相增强梯度涂层与活性元素改性梯度涂层。分析表明,梯度结构通过成分与物相沿厚度方向的阶梯过渡,有效缓解了钼基体与涂层间的热膨胀失配,并抑制了元素互扩散导致的脆性相析出;微量活性元素掺杂可在晶界偏聚、氧化膜改性与扩散阻挡等多维度提升涂层性能。当前涂层有效防护温度已覆盖1200-1700 °C,防护时间达数十至数百小时,但超高温硅耗尽、低温粉化氧化仍制约工程应用。多梯度复合设计、自修复等梯度设计有望进一步扩展其应用范围。

     

    Abstract: Molybdenum alloys undergo severe oxidation and material loss above 600 °C due to the volatilization of molybdenum trioxide (MoO3). Surface protective coatings are therefore essential for extending their high-temperature service life. However, the mismatch in thermal expansion coefficients between conventional oxidation-resistant coatings and molybdenum alloy substrates can lead to interfacial cracking. Accordingly, gradient oxidation-resistant coatings for molybdenum alloys are designed around three interrelated principles: thermal expansion matching, elemental diffusion control, and the formation and regeneration of protective scales, with the aim of achieving long-term coating stability.This paper reviews recent advances in gradient oxidation-resistant coatings for molybdenum alloys. Existing gradient coatings are classified within a two-level framework comprising five categories. The first level focuses on gradient-skeleton construction and includes stepwise diffusion gradient coatings, nanogradient coatings, and in-situ formed composite gradient coatings. The second level concerns composite modification of the gradient skeleton and includes second-phase-reinforced gradient coatings and active-element-modified gradient coatings. The analysis indicates that gradient structures, through stepwise transitions in composition and phase along the coating thickness, can effectively alleviate thermal expansion mismatch between the molybdenum substrate and the coating, while suppressing the formation of brittle phases caused by elemental interdiffusion. Trace active-element additions can further enhance coating performance through grain-boundary segregation, oxide-scale modification, and diffusion-barrier effects. Current coatings provide effective protection at temperatures ranging from 1200 to 1700 °C, with protection durations of tens to hundreds of hours. Nevertheless, silicon depletion at ultrahigh temperatures and pest oxidation at lower temperatures continue to limit their engineering applications. Multigradient composite architectures and self-healing strategies are expected to further expand the application range of these coatings.

     

/

返回文章
返回