AdvancedSearch

column
Investigation on Mechanical Alloying of Fe-Si System
Yang Junyou, Wu Jiansheng, Zeng Zhenpeng, Zhang Tongjun, Cui Kun
1997, 15(3): 165-168.
Abstract PDF
Study on Mechanical Properties of SiCw/ZTA(Y) Ceramic Composites
Jiang Yang, Xu Yufen
1997, 15(3): 169-173.
Abstract PDF
Effect of Forging Equipment Speed on plastic Deformation and Properties of Metal Powder Sintered Preform
Hong Shenzhang, Zhang Yi, Jiang Guanmin
1997, 15(3): 174-177.
Abstract PDF
The Effect of Swaging on Performance and Microstucture of 93W Alloy-Micro alloyed by Co、Mn
Zhou Guoan, Zhang Shouquan, Huang Jihua, Yang Minrang, Dong Jianwu
1997, 15(3): 178-181.
Abstract PDF
Effect of Clad on Diamond's Strength and Bond Capacity Between Diamond and Metal Matrix
Liu Xiongfei, Chen Peng
1997, 15(3): 182-185.
Abstract PDF
The Production of Nickel Powder with Nickel Sulphate Electrolyte Containing Low Chloride
Zhao Qijin, Li Rihui, Zhao Dehou, Dong Junqing
1997, 15(3): 186-189.
Abstract PDF
Manufacture of Fe-3Al2O3·2SiO2 Composite Green by In-situ Coagulation
Mu Bochun
1997, 15(3): 190-194.
Abstract PDF
Process of Bioceramic Coating with Laser-remelting Pretreatment
Gao Jiacheng, Zhang Yaping, Tang Hua
1997, 15(3): 195-198.
Abstract PDF
Continuous Production of Ultrafine Iron Powder
Sun Weimin, Jin Shouri
1997, 15(3): 199-202.
Abstract PDF
Microsturcture and Mechanical Properties of SiCp/Al Composites Made by Spray Co-deposition
Zhang Liying, Wu Chengyi, Lin Yaojun, Wang Rui
1997, 15(3): 203-207.
Abstract PDF
Influence of MoS2 and C on the Properites of P/M Diamond Composite Material
Wu Yikun, Yu Qing
1997, 15(3): 208-212.
Abstract PDF
Development in Valve of Auto Shock Absorbers
Wang Hongbing
1997, 15(3): 213-216.
Abstract PDF
Measurement of Sintered Steel's Fracture Toughness by Repeated Impact with Low Energy
Cao Shunhua, Xu Runze
1997, 15(3): 217-219.
Abstract PDF
Functional Structure Materials Prepared by Spray Co-deposition
Liu Yongzhang, Yang Gencang, Lü Yili
1997, 15(3): 220-222.
Abstract PDF