Combining electrostatic die wall lubrication and warm compaction to enhance green and sintered properties of P/M components[J]. Powder Metallurgy Technology, 2006, 24(3): 227-232. DOI: 10.3321/j.issn:1001-3784.2006.03.015
Citation:
|
Combining electrostatic die wall lubrication and warm compaction to enhance green and sintered properties of P/M components[J]. Powder Metallurgy Technology, 2006, 24(3): 227-232. DOI: 10.3321/j.issn:1001-3784.2006.03.015
|
Combining electrostatic die wall lubrication and warm compaction to enhance green and sintered properties of P/M components[J]. Powder Metallurgy Technology, 2006, 24(3): 227-232. DOI: 10.3321/j.issn:1001-3784.2006.03.015
Citation:
|
Combining electrostatic die wall lubrication and warm compaction to enhance green and sintered properties of P/M components[J]. Powder Metallurgy Technology, 2006, 24(3): 227-232. DOI: 10.3321/j.issn:1001-3784.2006.03.015
|