For the investigation of sintering kinetics, the surface area of sintered compacts is conventionally measured. The present paper outlines that the surface area of sintered porous metal for valve can be measured by anodic oxidation. Comparison was made between various calculating methods. It is concluded that better results can be obtained by oxygen equivalent method。