Preparation of SiC nanoparticles coated by ZnC2O4

More Information
  • Related Articles

    [1]REN Wei. Property characterization of Mn-Si powder porous alloy for semiconductors prepared by solid phase sintering[J]. Powder Metallurgy Technology, 2019, 37(6): 456-460. DOI: 10.19591/j.cnki.cn11-1974/tf.2019.06.009
    [2]YU Chong, YANG Jing, ZHANG Liang, LI Yuan-yuan, PAN Xiao-qiang. Preparation of nuclear-grade ZrB2 powders by sol-gel method[J]. Powder Metallurgy Technology, 2018, 36(5): 377-381. DOI: 10.19591/j.cnki.cn11-1974/tf.2018.05.010
    [3]FAN Lu, TONG Zhi, ZHANG Shuai, HUANG Wen-shuai, CHEN Fang-fang. Preparation and characterization of a TiO2-SiO2 composite membrane by sol-gel method[J]. Powder Metallurgy Technology, 2017, 35(2): 89-93. DOI: 10.3969/j.issn.1001-3784.2017.02.002
    [4]Huang Xiaohong, Ji Zhen, Jia Chengchang, Wang Zhaoli, Cheng Cheng, Liu Bowen. Preparation and characterization of paraffin microencapsulated phase change materials[J]. Powder Metallurgy Technology, 2015, 33(5): 347-350. DOI: 10.3969/j.issn.1001-3784.2015.05.006
    [5]Li Junyi, Wang Dongxin, Sun Benshuang, He Jilin, Guo Shun, Yang Guoqi. Characterization of ultrafine nickel powder for MLCC fabricated by coated precursor thermal decomposition method[J]. Powder Metallurgy Technology, 2013, 31(5): 360-364. DOI: 10.3969/j.issn.1001-3784.2013.05.008
    [6]Chen Chuang, Wei Shizhong, Zhou Zhihong, Zhang Guoshang, Li Jiwen, Xu Liujie. The process study of Al2O3/Mo nano powder preparation by sol-gel method[J]. Powder Metallurgy Technology, 2013, 31(2): 108-113,118. DOI: 10.3969/j.issn.1001-3784.2013.02.005
    [7]Lu Ping, Shen Chunying, Qiu Tai. Preparation of tungsten nano-powder doped with CeO2 by sol-gel method[J]. Powder Metallurgy Technology, 2008, 26(6): 455-458.
    [8]Li Yue, Ye Hongqi, Liu Hui. Preparation of flaky TiO2 powders by a novel method[J]. Powder Metallurgy Technology, 2008, 26(5): 354-359.
    [9]Cui Sheng, Shen Xiaodong, Xiao Su, Gao Zhiqiang. Preparation of Cu coated SiC nanoparticles by electroless plating method[J]. Powder Metallurgy Technology, 2008, 26(4): 281-285,290.
    [10]Wang Tiejun, Wang Shenghong. SiC Powder Manufactured by Preheating SHS[J]. Powder Metallurgy Technology, 1997, 15(2): 106-109.

Catalog

    Article Metrics

    Article views (217) PDF downloads (9) Cited by()
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return