1988年  第6卷  第1期

专题论述
THE SYNTHESIS OF HIGH TEMPERATURE MATERIALS BY SELF-PROPAGATING COMBUSTION METHODS
Z.A. Munir
1988, 6(1): 1-23.
摘要:
The Process of Splf-Propagating High-temperature Synthesis(SHS) is reviewed as a method for the preparation of high temperature materials. A broad description of the fundamental aspects of this process is provided along with a historical account of its utilization in materials synthesis. Advantages and limitations of the process are discussed with specific reference to selected classes of materials. The use of the SHS process to produce dense bodies is described.
研究与试验
等离子喷涂钴包碳化钨涂层显微结构的研究
周序科, 闻立时, 关侃
1988, 6(1): 25-31.
摘要:
利用x—衍射、扫描电镜、透射电镜、金相等物理实验方法,研究了低压等离子和大气等离子喷涂钴包碳化钨涂层的显微组织结构,并讨论了致密化机理。
工艺与设备
粉末轧制多孔不锈钢薄壁焊接管材的研究
郭栋, 李德泉, 王恩珂
1988, 6(1): 32-36.
摘要:
本文研究了用不锈钢粉末轧制多孔生带材,经烧结、卷曲和焊接等工艺生产多孔管材的方法。粒度大于5mm的气体雾化不锈钢丸经涡旋研磨机破碎成粒度组成为-100+250目的不锈钢粉末,再用上述工艺获得壁厚为0.8-1.2mm的多孔不锈钢管。其相对渗透性可达(3~7)×10-3L·N/cm2·min·mmH2O,平均孔径为6-15μm。
氢一次还原钨粉烧结多孔构件的工艺研究
孙百顺
1988, 6(1): 37-42.
摘要:
研究了氢一次还原、平均粒度为6.5—7.5μm的钨粉的烧结特性。得出多孔钨构件的相对密度随烧结温度和时间、粉末粒度、压制件密度而变化的规律。提出了生产相对密度为78—81%、开孔率>95%的多孔钨的生产工艺参数,即:压制件相对密度为60—65%,烧结温度为2100—2250℃、时间为4—8小时。
气雾化6-6-3青铜粉的粒度组成对松装密度及压缩性的影响
王守时, 张辉
1988, 6(1): 43-46.
摘要:
本文简述了气雾化6-6-3青铜粉末的粒度对松装密度、流速及压缩性的影响。表明,粉末细颗粒(-320+400目)越乡,松装密度越大;粗颗粒越多,流速越快;细颗粒在70%左右时,其压件密度最大。
含油轴承自动割槽机
陈乔
1988, 6(1): 47-51,24.
摘要:
带挡边粉末冶金含油轴承的退刀槽及挡边里平面,常需通过切削加工制得。本文介绍的自动割槽机能自动完成带挡边青铜含油轴承的车边切槽工序。自动割槽机由床身及主轴部件、送料部件、夹紧部件和刀架部件构成,执行机构的工作程序由凸轮进行控制。与原来的手工割槽相比,无论加工质量还是产量都有大幅度的提高,尤其是减轻了工人的劳动强度,确保了安全生产,因此该机床受到了操作工人的欢迎。
材料·制品·应用
烧结高速钢及其应用
戴行仪, 严建肃, 仲守亮, 刘云美
1988, 6(1): 52-57,42.
摘要:
烧结致密法是制取高性能粉末冶金工具钢制品的一个途径。应用该工艺可获得基本致密,性能较高的粉末冶金工具钢材料。本文简述烧结高速钢制品的基本生产工艺及其性能。初步应用表明,它在切削工具、模具及耐磨件中的应用前景良好。
新型铜石墨基和银基触头配对使用的节银效果
李业建
1988, 6(1): 58-62.
摘要:
本文研究新型非对称性触头在DW10-400框架式断路器上的使用情况,并对其经济效果作了分析。表明,所选择的非对称性触头的使用性能优于原使用的Ag—W自配对触头,完全满足电器产品的技术要求,并比原用触头节银50%。