Process optimizing and experimental validation of irregular thick-wall tubular billet prepared with reciprocating multi-layers spray forming

  • 摘要: 提出了基于往复式喷射成形工艺制备大璧厚非规则管坯的近终形成形工艺及其工艺参数优化方法,以实现坯件从CAD设计到喷射成形的快速制备过程.该工艺方法包括三个阶段:非规则管坯的三维CAD设计、分层处理和单层沉积厚度计算;基于沉积厚度与往复速度和质量流率的对应关系,计算满足各层沉积厚度所对应的控制参数;利用控制系统和执行机构对控制参数进行实时控制和调节,采用往复式多层喷射成形工艺制备满足设计轮廓的管坯.通过试验进行了验证,喷射成形制备的管坯形状和轮廓与CAD设计模型较好地一致,表明了该工艺方法的可行和正确性.