Zhang Long, Zhao Zhongmin, Cao Jinrong, Lu Daqin, Wang Jianjiang. Influences of metallic additive on microstructures and interface-bonding of ceramic-lined composite pipes fabricated by the SHS process[J]. Powder Metallurgy Technology, 2005, 23(4): 248-253. doi: 10.3321/j.issn:1001-3784.2005.04.002
Citation: Zhang Long, Zhao Zhongmin, Cao Jinrong, Lu Daqin, Wang Jianjiang. Influences of metallic additive on microstructures and interface-bonding of ceramic-lined composite pipes fabricated by the SHS process[J]. Powder Metallurgy Technology, 2005, 23(4): 248-253. doi: 10.3321/j.issn:1001-3784.2005.04.002

金属添加剂对SHS陶瓷内衬复合管微观结构与界面连接的影响

doi: 10.3321/j.issn:1001-3784.2005.04.002
基金项目: 中国科学院资助项目(59972043)%军械工程学院校科研和教改项目(YJJXM02013)
详细信息
  • 中图分类号: TF12

Influences of metallic additive on microstructures and interface-bonding of ceramic-lined composite pipes fabricated by the SHS process

  • 摘要: 基于重力分离SHS法制备陶瓷内衬复合管,以(CrO3+Al)为燃烧体系,通过添加并调整(TiO2+Al+C)子体系与Ni金属添加剂之间的成分比例, 合成出具有钢基体、中间过渡合金层与内衬陶瓷三层结构的复合管.研究金属添加剂Ni对燃烧行为、碳化物颗粒原位合成与分布、陶瓷/金属微连接及复合管力学性能的影响. 研究发现,随着Ni添加量增多与(TiO2+Al+C)含量降低,反应体系的绝热燃烧温度与燃烧速率上升,Ni的添加与熔化促进反应中亚化学计量比的富Ti碳化物形成,同时也因液相传质促进该碳化物溶解于金属熔体中,并经结晶形成呈梯度分布于中间过渡合金层上的富Ti碳化物.经对复合管力学性能测试与SEM观察,发现添加适量的Ni粉,可以控制中间过渡合金层中碳化物的体积分数与分布,有利于内衬陶瓷层、中间过渡合金层与钢基体之间的连接,从而使复合管径向压溃强度与抗剪强度提高.