铁精矿粉粒度对精控还原工艺的影响

李玉柱 姜丽娟 柳学全 李发长 李一 李楠

李玉柱, 姜丽娟, 柳学全, 李发长, 李一, 李楠. 铁精矿粉粒度对精控还原工艺的影响[J]. 粉末冶金技术, 2016, 34(2): 119-124. doi: 10.3969/j.issn.1001-3784.2016.02.008
引用本文: 李玉柱, 姜丽娟, 柳学全, 李发长, 李一, 李楠. 铁精矿粉粒度对精控还原工艺的影响[J]. 粉末冶金技术, 2016, 34(2): 119-124. doi: 10.3969/j.issn.1001-3784.2016.02.008
Li Yuzhu, Jiang Lijuan, Liu Xuequan, Li Fachang, Li Yi, Li Nan. Effect of particle size of fine iron ore concentrate powder on fine control reduction process[J]. Powder Metallurgy Technology, 2016, 34(2): 119-124. doi: 10.3969/j.issn.1001-3784.2016.02.008
Citation: Li Yuzhu, Jiang Lijuan, Liu Xuequan, Li Fachang, Li Yi, Li Nan. Effect of particle size of fine iron ore concentrate powder on fine control reduction process[J]. Powder Metallurgy Technology, 2016, 34(2): 119-124. doi: 10.3969/j.issn.1001-3784.2016.02.008

铁精矿粉粒度对精控还原工艺的影响

doi: 10.3969/j.issn.1001-3784.2016.02.008
基金项目: 国家高技术研究计划(863计划)(2013AA031102)

Effect of particle size of fine iron ore concentrate powder on fine control reduction process

  • 摘要: 本文以河北承德地区的铁精矿粉为原料,选用模拟隧道窑还原工艺制备海绵铁粉,研究了铁精矿粉粒度对精控还原工艺的影响.结果表明:铁精矿粉粒度对其还原工艺影响很大,并直接影响海绵铁粉的产品性能.在既定试验条件下,随着铁精矿粉粒度的增大,其精控还原所需最优还原温度随着增加,最佳配碳量先减少后增大,而最佳还原时间随粒度的增大呈现出先增大后减小的变化趋势.究其原因为粒度过小导致的粉体烧结和粒度过大导致的粉体芯部不易还原均会阻碍还原过程的进行.45~75 μm粒度区间铁精矿粉最适合作为制备优质海绵铁粉原料,其在配碳量0.8、还原温度1 150℃、还原时间4.5h的精控还原工艺下可制得的海绵铁粉的铁含量高达97.88%.