纳米Mo-Cu超饱和固溶体粉的结构特征及其烧结机制

陈玉柏 范景莲 刘涛 韩勇 陈旭

陈玉柏, 范景莲, 刘涛, 韩勇, 陈旭. 纳米Mo-Cu超饱和固溶体粉的结构特征及其烧结机制[J]. 粉末冶金技术, 2016, 34(4): 258-263. doi: 10.3969/j.issn.1001-3784.2016.04.004
引用本文: 陈玉柏, 范景莲, 刘涛, 韩勇, 陈旭. 纳米Mo-Cu超饱和固溶体粉的结构特征及其烧结机制[J]. 粉末冶金技术, 2016, 34(4): 258-263. doi: 10.3969/j.issn.1001-3784.2016.04.004
Chen Yubo, Fan Jinglian, Liu Tao, han Yong, Chen Xu. Structure characteristics and sintering mechanism of nano Mo-Cu supersaturated solid solution powders[J]. Powder Metallurgy Technology, 2016, 34(4): 258-263. doi: 10.3969/j.issn.1001-3784.2016.04.004
Citation: Chen Yubo, Fan Jinglian, Liu Tao, han Yong, Chen Xu. Structure characteristics and sintering mechanism of nano Mo-Cu supersaturated solid solution powders[J]. Powder Metallurgy Technology, 2016, 34(4): 258-263. doi: 10.3969/j.issn.1001-3784.2016.04.004

纳米Mo-Cu超饱和固溶体粉的结构特征及其烧结机制

doi: 10.3969/j.issn.1001-3784.2016.04.004

Structure characteristics and sintering mechanism of nano Mo-Cu supersaturated solid solution powders

  • 摘要: 采用溶胶-喷雾干燥-煅烧-氢还原方法制备了纳米Mo-Cu复合粉末.综合利用XRD、TEM和EDX等检测方法对该Mo-Cu复合粉末的相结构特征和粉末体的烧结机制进行了分析.结果说明:纳米Mo-Cu复合粉末由Mo(Cu)和Cu (Mo)超饱和固溶体组成,但该Mo(Cu)和Cu (Mo)超饱和固溶体呈不稳定状态,随烧结温度升高和保温时间延长,固相Mo(Cu)中析出的Cu逐渐溶解于液相Cu (Mo)中,而液相Cu (Mo)中的Mo逐渐析出沉积在固相Mo(Cu)颗粒上,此过程促进了烧结体致密化.